Properties
Relationship with standards and mechanical properties
The values shown for the mechanical properties in the table below are for test pieces taken longitudinal to the rolling direction.
Tata Steel grade |
|
Ymagine®70 XF |
ASTM A 1011: 2007 |
Hot-rolled flat products |
HSLAS-F grade 70 |
Yield strength |
ksi |
≥ 70 |
Tensile strength |
ksi |
≥ 80 |
Elongation |
% |
≥ 18 |
Tata Steel grade |
|
Ymagine® 70 XF |
ASTM A 1008: 2013 |
Cold-rolled flat products |
HSLAS-F grade 70 |
Yield strength |
ksi |
≥ 70 |
Tensile strength |
ksi |
≥ 80 |
Elongation (2 inch) |
% |
≥ 16 |
Tata Steel grade |
Direct-rolled flat products |
Ymagine® 70 XF |
|
|
Typical value |
Guaranteed values |
Yield strength |
ksi |
78 |
70 - 95 |
Tensile strength |
ksi |
90 |
80 - 105 |
Elongation (2 inch) |
% |
22 |
≥ 16 |
Min. Elongation after fracture uses test piece length L0 is 2 inches.
Please contact us for further information on Charpy toughness and impact test properties.
Chemical composition
Heat analysis in weight percentages.
Tata Steel grade |
Ymagine® 70 XF |
|
Typical |
Guaranteed (max) |
C |
0.045 |
0.075 |
Mn |
0.800 |
1000 |
P |
0.009 |
0.020 |
S |
0.006 |
0.010 |
Si |
0.020 |
0.035 |
Cb |
0.015 |
0.020 |
V |
0.130 |
0.150 |
For the purpose of batch galvanizing, Ymagine® high-strength steels can be ordered on consultation with a maximum Si content of 0.030%..